Isolator Thickness Effect on Galvanic Corrosion Mitigation

Model ID: 13861


The use of Aluminum (Al) isolator is a commonly employed mitigation strategy for galvanic corrosion between magnesium alloy (Mg) and mild steel (MS). The present model demonstrates the effect of Al isolator thickness on galvanic corrosion severity using a parametric study. The electrode kinetics is implemented here using the experimental polarization data available in literature.

This model was built using the following:

Corrosion Module